DX53D Galvanized Steel Coil is a hot dip galvanized steel product produced under EN 10346 standard, specifically developed for deep drawing and complex forming applications. The steel combines excellent ductility with a durable zinc coating that offers long-term corrosion protection. Its regular spangle surface is formed naturally during galvanizing, giving the material both a distinctive metallic appearance and stable coating performance.

 

In the automotive industry, DX53D Regular Spangle Galvanized Steel Coil has become a preferred material for manufacturing structural components, interior panels, reinforcement parts, and numerous safety-related assemblies.

 

Galvanized Steel Coil

Specifications of DX53D Galvanized Steel Coil

 

EN 10346
DX53D
0.30 – 3.00 mm
600 – 1500 mm
Z100 – Z275 g/m²

 

 

140 – 220 MPa
270 – 350 MPa
>= 36%

 

Automotive manufacturing requires materials that provide consistent forming behavior, minimal defect rates, and excellent durability. DX53D Regular Spangle Galvanized Steel Coil delivers all three advantages through:

 

These characteristics help reduce scrap rates, extend tool life, and ensure dimensional stability in large-scale production.

 

Key Automotive Applications of DX53D

 

DX53D Regular Spangle Galvanized Steel Coil is extensively used in:

Its corrosion-resistant coating ensures long service life even under aggressive environmental conditions.

 

 

DX53D Galvanized Steel
22–28% >= 36%

Manufacturers using DX53D Regular Spangle Galvanized Steel Coil often report production efficiency improvements of 15–25% due to reduced defect rates and improved forming consistency.

 

Automotive components are constantly exposed to moisture, salt spray, and temperature fluctuations. The zinc coating of DX53D Regular Spangle Galvanized Steel Coil forms a sacrificial protection layer that prevents rust from penetrating the base metal, even when minor surface damage occurs.

This ensures extended vehicle lifespan and lower long-term maintenance costs.

 

DX53D supports sustainable manufacturing by:

These factors make DX53D not only a technical solution but also a financially and environmentally responsible material choice.

 

 

Elongation A80 (min %) r90 (min) n90 (min)
DX51D EN 10346 - 270 – 500 22 - -
DX52D EN 10346 140 – 300 ²) 270 – 420 26 - -
DX53D EN 10346 140 – 260 270 – 380 30 - -
DX54D EN 10346 120 – 220 260 – 350 36 1.6 ⁴) 0.18
DX56D EN 10346 120 – 180 260 – 350 39 1.9 ⁵) 0.21 ⁵)
DX57D EN 10346 120 – 170 260 – 350 41 2.1 ⁵) 0.22

 

GNEE STEEL supplies DX53D Galvanized Steel Coil with consistent quality, precise dimensional control, and stable global delivery. With strict quality management systems and advanced production lines, GNEE STEEL ensures every coil meets international automotive manufacturing standards.

 

From initial inquiry to final shipment, GNEE STEEL provides professional technical support, competitive pricing, and customized solutions for automotive manufacturers worldwide.

 

Contact GNEE STEEL today for detailed specifications and a competitive quotation.

 

A szálláslekérdezés elküldése

A szálláslekérdezés elküldése